Roof and wall cladding, supplied with the frame it fits
Cladding is where a steel building leaks, sweats or burns. The panel core sets the fire class, the coating sets the life, and the details set whether it leaks. We size purlins and girts for the panel you choose and supply the flashings from the same model.
Sandwich panels are covered by EN 14509; reaction to fire is classed to EN 13501-1.
Core
Reaction to fire (typical)
Fire resistance
Thermal conductivity
PUR (polyurethane)
D-s3,d0 to B-s3,d0
Rendah
0.023 W/m·K
PIR (polyisocyanurate)
C-s1,d0 to B-s1,d0
Limited
0.018 W/m·K
Stone wool
A2-s1,d0, non-combustible
Up to EI 240 by thickness
0.039 W/m·K
Values from a stone wool panel manufacturer’s technical guide; the exact class is on each product’s declaration of performance. Insurers may also require FM 4880 approval.
Aturan praktis: PIR insulates best per millimetre; stone wool is the only core that is non-combustible. Fire walls and plants with strict fire codes usually need stone wool.
By climate
What changes in hot, humid and coastal sites
Hot climates
Reflective coatings and insulation cut heat gain; ridge vents release hot air.
Humid tropics
A continuous vapour control layer stops condensation dripping on goods.
Coastal sites
AZ150 or higher metallic coating and PVDF top coats resist salt.
From our engineers
Where steel roofs leak, and how we detail them
Laps on low slopes. Through-fixed sheet needs enough slope and sealed laps. Below about 5° we recommend standing seam.
Penetrations. Every pipe and fan through the roof is a leak path. Group them and use factory flashings.
Gutters. Box gutters are sized for local rainfall intensity with overflows, not just to match the eave.
Thermal movement. Long sheets expand. Fixings and clips allow it, or fasteners loosen and leak.